Welcome to our websites!

YYP-HP5 Differential scanning calorimeter

Short Description:

Parameters:

  1. Temperature range: RT-500℃
  2. Temperature resolution:0.01℃
  3. Pressure range: 0-5Mpa
  4. Heating rate: 0.1~80℃/min
  5. Cooling rate: 0.1~30℃/min
  6. Constant temperature: RT-500℃,
  7. Duration of constant temperature: The duration is recommended to be less than 24 hours.
  8. DSC range: 0~±500mW
  9. DSC resolution: 0.01mW
  10. DSC sensitivity: 0.01mW
  11. Working power: AC 220V 50Hz 300W or other
  12. Atmosphere control gas: Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen)
  13. Gas flow:0-200mL/min
  14. Gas pressure:0.2MPa
  15. Gas flow accuracy: 0.2mL/min
  16. Crucible: Aluminium crucible Φ6.6*3mm (Diameter * High)
  17. Data interface: Standard USB interface
  18. Display mode: 7-inch touch screen
  19. Output mode: computer and printer

Product Detail

Product Tags

Summary

This item is a touch screen type, specially testing polymer material oxidation induction period test, customer one

key operation, software automatic operation.

Conforming the following standards:

GB/T 19466.2- 2009/ISO 11357-2:1999

GB/T 19466.3- 2009/ISO 11357-3:1999

GB/T 19466.6- 2009/ISO 11357-6:1999 ASTM D3895

ASTM D5885

Features

Industrial level widescreen touch structure is rich in information, including setting temperature, sample temperature, oxygen flow, nitrogen flow, differential thermal signal, various switch states, etc.

USB communication interface, strong universality, reliable communication, support self-restoring connection function.

The furnace structure is compact, and the rate of rising and cooling is adjustable.

The installation process is improved, and the mechanical fixation method is adopted to completely avoid the contamination of the internal colloidal of the furnace to the differential heat signal.

The furnace is heated by heating wire, compact structure and small size.

The double temperature probe ensures the high repeatability of the sample temperature measurement, and adopts the special temperature control technology to control the temperature of the furnace wall to set the

temperature of the sample.

The gas flow meter automatically switches between two channels of gas, with fast switching speed and short stable time.

Standard sample is provided for easy adjustment of temperature coefficient and enthalpy value coefficient.

Software support each resolution screen, automatically adjust the computer screen size curve display mode. Support laptop, desktop; Support Win2000, XP, VISTA, WIN7, WIN8, WIN10 and other operating systems.

Support user edit device operation mode according to actual needs to achieve full automation of measurement steps. The software provides dozens of instructions, and users can flexibly combine and save each instruction according to their own measurement steps. Complex operations are reduced to one-click operations.

Parameters

1.Temperature range: RT-500℃

2.Temperature resolution:0.01℃

3.Pressure range: 0-5Mpa

4.Heating rate: 0.1~80℃/min

5.Cooling rate: 0.1~30℃/min

6.Calorimetric resolution: 100%. Under certain conditions, the two approximate thermal effects can be completely distinguished

7.Constant temperature: RT-500℃

8.Duration of constant temperature: The duration is recommended to be less than 24 hours.

9.Temperature control mode: Heating, cooling, constant temperature, any combination of three modes cycle use, temperature uninterrupted

10.DSC range: 0~±500mW

11.DSC resolution: 0.01mW

12.DSC sensitivity: 0.01mW

13.Working power: AC 220V 50Hz 300W or other

14.Atmosphere control gas: Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen)

15.Gas flow:0-200mL/min

16.Gas pressure:0.2MPa

17.Gas flow accuracy: 0.2mL/min

18.Crucible: Aluminium crucible Φ6.6*3mm (Diameter * High)

19.Calibration standard: with standard material (indium, tin, zinc), users can adjust the temperature coefficient  and enthalpy value coefficient by themselves

20.Data interface: Standard USB interface

21.Display mode: 7-inch touch screen

22.Output mode: computer and printer

23.Fully closed support structure design, prevent items falling into the furnace body, pollution of the furnace body, reduce the maintenance rate

Configuration list

1.A DSC machine

2.300 Aluminium crucibles

3.A power cords and a USB cable

4.A CD (contains software and operations video)

5.A Soft-key

6.Oxygen airway and nitrogen airway, each 5m

7.A operation manual

8.A Standard sample(contains Indium, tin, zinc)

9.A tweezer and a medicine spoon

10.2 pairs of custom pressure reducing valve joint and quick joint

11.4 fused glass fuses

Software screenshots

printer1 printer2 printer3 printer4 printer5




  • Previous:
  • Next:

  • Write your message here and send it to us