YYP-P600 Differential Scanning Calorimeter

Short Description:

Summary:

Various thermodynamic and kinetic parameters are measured, such as specific heat capacity, enthalpy, melting and curing, glass transition temperature, crystallization rate, polymer crystallinity, sample purity, etc. It is applicable to inorganic substances, organic substances, polymer compounds and drug analysis.

 

Complies with but is not limited to the following standards:

1. ISO 11357-2:2020 Plastics Part 2: Determination of glass transition temperature and step height

2. ISO 11357-3:2025 Plastics Part 3: Determination of temperature and enthalpy of melting and crystallization

3. ISO 11357-6:2025 Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT)

4. ASTM D3895-14 Standard Test Method for Oxidative-Induction Time of Polyolefins by DSC

5. ASTM D6580-17 Standard Test Method for the Determination of Metallic Zinc Cont

6. ISO 21809-2:2014 External coatings for buried or submerged pipelines used in pipeline transportation systems- Part 2: Single layer fusion-bonded epoxy coatings

7. ISO 14322:2018 Plastics-Epoxy resins-Determination of degree of crosslinking of crosslinked epoxy resins by DSC

8. ISO 15874-2:2013 Plastics piping systems for hot and cold water installations – Polypropylene (PP) Part 2: Pipes

 

Features:

1. Industrial level widescreen touch structure is rich in information, including setting temperature, sample temperature, differential thermal signal, various switch states, etc.

2. Gigabit Ethernet, strong universality, reliable communication, support self-restoring connection function.

3. The furnace structure is compact, and the rate of rising and cooling is adjustable.

4. The installation process is improved, and the mechanical fixation method is adopted to completely avoid the contamination of the internal colloidal of the furnace to the differential heat signal.

5. The furnace is heated by heating wire, compact structure and small size.

6. The double temperature probe ensures the high repeatability of the sample temperature measurement, and adopts the special temperature control technology to control the temperature of the furnace wall to set the temperature of the sample.

7. The gas flow meter automatically switches between two channels of gas, with fast switching speed and short stable time.

8. Standard sample is provided for easy adjustment of temperature coefficient and enthalpy value coefficient.

9. Software support each resolution screen, automatically adjust the computer screen size curve display mode. Support laptop, desktop; SupportWIN7 64bit, WIN10, WIN11.

10. Support user edit device operation mode according to actual needs to achieve full automation of measurement steps. The software provides dozens of instructions, and users can flexibly combine and save each instruction according to their own measurement steps. Complex operations are reduced to one-click operations.


Product Detail

Product Tags

Parameters:
1. Temperature range: RT~600℃
2. Temperature resolution:0.01℃
3. Enthalpy variable precision: ±2%△H
4. Heating rate: 0.1~100℃/min
5. Cooling rate: 0.1~30℃/min (Constant cooling at 10℃/min, applicable range from 550℃ to 100℃)
6. Constant temperature: RT~500℃
7. Duration of constant temperature: The duration is recommended to be less than 24 hours.
8. Temperature control mode: Heating, cooling, constant temperature, any combination of three modes cycle use, temperature uninterrupted
9. DSC range: 0~±3000mW
10. DSC resolution: 0.0001mW(0.1uW)
11. Time resolution:0.2s
12. Working power: AC 220V 50Hz 300W or other
13. Atmosphere control gas: Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen)
14. Gas flow:20~200mL/min
15. Gas pressure:0.2MPa
16. Crucible: Aluminum crucible Φ6.5*3mm (Diameter * High)
17. Calibration standard: with standard material (indium, tin, zinc), users can adjust the temperature coefficient and enthalpy value coefficient by themselves
18. Data interface: Gigabit Ethernet
19. Display mode: 10-inch touchscreen in Chinese, English, or Russian   